WOVEN GEO-TEXTILES
110 GRAM PER SQUARE METER
Minimum Average Roll Values when tested in accordance with the ASTM methods listed below.
Property |
Test Method |
Imperial |
Metric |
Grab Tensile Strength |
ASTM D-4632 |
135 lbs |
590 N |
Elongation |
ASTM D-4632 |
18 % |
18 % |
Puncture |
ASTM D-4833 |
90 lbs |
396 N |
Mullen Burst |
ASTM D-3786 |
350 psi |
2408 kpa |
Trapezoidal Tear |
ASTM D-4533 |
80 lbs |
352 N |
UV Resistance (retained after 1200 hrs) |
ASTM D-4355 |
70 % |
70 % |
Apparent Opening Size |
ASTM D-4751 |
30 US Sieve |
0.60 mm |
Permittivity |
ASTM D-4491 |
0.05 sec-1 |
0.05 sec-1 |
Flow Rate |
ASTM D-4491 |
4 gpm/m2 |
163 lpm/m2 |
Seller makes no warranty, expressed or implied, concerning the product furnished hereunder other than at the time of delivery it shall be of the quality and specification stated herein.